摘要

采用碳酸盐共沉淀法合成了均相Li_(1.4)[Ni_(0.15)Co_(0.15)Mn_(0.7)]O_(2.475)和{[Ni_(1/6)Co_(1/6)Mn_(4/6)]0.7core[Ni_(0.14)Co_(0.14)Mn_(0.72)]0.1shel 1[Ni_(0.115)Co_(0.115)Mn_(0.77)]_(0.1) shel 2[Ni_(0.09)Co_(0.09)Mn_(0.82)]_(0.1shel3)}CO_3多级核壳结构锂离子电池富锂正极材料。通过X射线粉末衍射分析(XRD)、扫描电镜测试(SEM)、粒度分析和电化学性能测试对所得样品的结构、形貌、粒度和电化学性能...