广西某含碳难选铅锌矿含铅3.68%,锌6.76%,银58.24克/吨,碳3.65%,铅氧化率为38.04%。研究采用碳铅混浮-选锌优先浮选工艺、铅浮选新型捕收剂,获得了较好的选矿指标:铅精矿铅品位50.12%,锌品位5.34%,银品位744.0g/t,铅回收率70.01%;锌精矿锌品位53.98%,铅品位2.28%,银品位107.09g/t,锌回收率89.18%。